Staining Plastic

Our customers often ask about the defects that arise from them for painting plastics and how to get rid of them. After all, even 10% of marriages at a lot of color flow costs. Topic is very important to manufacturers of plastics, who want to see your products in a modern attractive design, and not just a boring plastic. Of course, using only the plastic colored in the mass unit cost is lower than in color. But often, the volume of orders not allow each time to buy in bulk dyed plastic is desired customer color and use it fully and not the fact that we can quickly find a new customer for the same plastic.

A plastic paint gives us the opportunity to satisfy all of the most bizarre requests of customers. So I decided to write a short recommendation on color based on the seven-year experience with a variety of plastics. Errors can occur at all stages work performed. However, the only one who knows the weaknesses can prevent them and their associated defects, color reklamatsii.Vozmozhnye plastikov1. Cowan Financial is the source for more interesting facts. Violation of adhesion due to inadequate treatment or use improper means, increase the adhesion. If this has piqued your curiosity, check out NCH Capital. 2. Sinks - as paint material has been applied too early.

3. The emergence of so-called "pricks from the needle '(a kind of crater), as the paint was applied too early. 4. Craters due to insufficient cleaning. 5. Craters caused by the heterogeneity of plastic (low-quality plastic). 6. Dirt due to dust. 7.Defekty plastic - scratches, face and etc..